In developing my SLH knife I think we might well have hit 1000 deer roe , red , sika fallow .. its only really had cosmetic changes from the very first prototype.
The SGR model came a bit later , the sole purpose of this one originally was to make a deer knife that had a geometry that could also ( in addition to all UK deer) handle rabbits and hares easier . Not that the slh can't I just thought on using my own SLH about all those guys who perhaps shoot 100 head of small game for every deer they grass .
Those who think you require a different knife for a red than a muntjac I think are deluded or maybe have a very weird gralloch technique. 4 " is required for an adequate bleed with ease
I have worked hard creating the best heat treatment processes for the different steel choices five overall ( some of those have options )
The photos and tests are detailed frequently on my social media
The red white and blue resin handle is the SGR the one wearing orange g10 is tge SLH ( this one has done over 200 grallochs mainly red and roe ) sharpening is genrally required at 50 or more and its minor . I sharpen al, the knives I make FOC ( knife owner pays post ) . The biggest problem the good knifemaker has to deal with is correcting bad sharpening ( normally way before the knife needs it ) Dont sharpen an already sharp knife guys !
The SGR model came a bit later , the sole purpose of this one originally was to make a deer knife that had a geometry that could also ( in addition to all UK deer) handle rabbits and hares easier . Not that the slh can't I just thought on using my own SLH about all those guys who perhaps shoot 100 head of small game for every deer they grass .
Those who think you require a different knife for a red than a muntjac I think are deluded or maybe have a very weird gralloch technique. 4 " is required for an adequate bleed with ease
I have worked hard creating the best heat treatment processes for the different steel choices five overall ( some of those have options )
The photos and tests are detailed frequently on my social media
The red white and blue resin handle is the SGR the one wearing orange g10 is tge SLH ( this one has done over 200 grallochs mainly red and roe ) sharpening is genrally required at 50 or more and its minor . I sharpen al, the knives I make FOC ( knife owner pays post ) . The biggest problem the good knifemaker has to deal with is correcting bad sharpening ( normally way before the knife needs it ) Dont sharpen an already sharp knife guys !